http://www.cnr.it/ontology/cnr/individuo/prodotto/ID43432
Microstructure and mechanical properties of ZrB2-MoSi2 ceramic composites produced by different sintering techniques (Articolo in rivista)
- Type
- Label
- Microstructure and mechanical properties of ZrB2-MoSi2 ceramic composites produced by different sintering techniques (Articolo in rivista) (literal)
- Anno
- 2006-01-01T00:00:00+01:00 (literal)
- Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#doi
- 10.1016/j.msea.2006.06.112 (literal)
- Alternative label
Diletta Sciti; Frédéric Monteverde; Stefano Guicciardi; Giuseppe Pezzotti; Alida Bellosi (2006)
Microstructure and mechanical properties of ZrB2-MoSi2 ceramic composites produced by different sintering techniques
in Materials science & engineering. A, Structural materials: properties, microstructure and processing
(literal)
- Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#autori
- Diletta Sciti; Frédéric Monteverde; Stefano Guicciardi; Giuseppe Pezzotti; Alida Bellosi (literal)
- Pagina inizio
- Pagina fine
- Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#url
- http://www.sciencedirect.com/science/article/pii/S0921509306012603 (literal)
- Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#numeroVolume
- Rivista
- Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#pagineTotali
- Note
- ISI Web of Science (WOS) (literal)
- Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#affiliazioni
- D. Sciti, F. Monteverde, S. Guicciardi, A. Bellosi (CNR-ISTEC, Institute of Science and Technology for Ceramics, Via Granarolo 64, I-48018 Faenza, Italy), G. Pezzotti (Department of Chemistry and Materials Technology, Kyoto Institute of Technology, Sakyo-ku, Matsugasaki, 606-8585 Kyoto, Japan) (literal)
- Titolo
- Microstructure and mechanical properties of ZrB2-MoSi2 ceramic composites produced by different sintering techniques (literal)
- Abstract
- Ceramic composites in the system ZrB2-(15-20 vol% MoSi2) were produced by different densification techniques: pressureless sintering, hotpressing and spark plasma sintering. Regardless of the sintering technique, the addition of 15-20 vol% MoSi2 was beneficial for the densification of these composites. Nearly fully dense materials (98-99%) were obtained at 1750-1800 °C by the pressure-assisted techniques and at 1850 °C by pressureless sintering. All the microstructures were very fine, with mean ZrB2 grain sizes between 1.4 and 2.5 micrometers. Vickers hardness, fracture toughness, Young's modulus and CTEs were similar for all the materials produced. The room temperature flexural strength varied between 500 and 700 MPa. At 1200 and 1500 °C, the highest values of flexural strength were obtained for the pressureless sintered material (655 and 500 MPa, respectively). The high-temperature flexural strength of the hot-pressed and spark plasma sintered samples was negatively affected by residual silica pockets. (literal)
- Prodotto di
- Autore CNR
- Insieme di parole chiave
Incoming links:
- Prodotto
- Autore CNR di
- Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#rivistaDi
- Insieme di parole chiave di