Variations in the lifetime of 3d hole states in ultrathin Fe films grown on Cu(100) deduced from the LMM Auger spectra of Fe (Articolo in rivista)

Type
Label
  • Variations in the lifetime of 3d hole states in ultrathin Fe films grown on Cu(100) deduced from the LMM Auger spectra of Fe (Articolo in rivista) (literal)
Anno
  • 2002-01-01T00:00:00+01:00 (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#doi
  • 10.1142/S0218625X02002877 (literal)
Alternative label
  • S. D'Addato, P. Luches, R. Gotter, L. Floreano, D. Cvetko, A. Morgante, A. Newton, D. Martin, P. Unsworth, P. Weightman (2002)
    Variations in the lifetime of 3d hole states in ultrathin Fe films grown on Cu(100) deduced from the LMM Auger spectra of Fe
    in Surface review and letters; World Scientific Publishing Co. Pte. Ltd., Singapore (Singapore)
    (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#autori
  • S. D'Addato, P. Luches, R. Gotter, L. Floreano, D. Cvetko, A. Morgante, A. Newton, D. Martin, P. Unsworth, P. Weightman (literal)
Pagina inizio
  • 709 (literal)
Pagina fine
  • 716 (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#numeroVolume
  • 9 (literal)
Rivista
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#pagineTotali
  • 8 (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#numeroFascicolo
  • 2 (literal)
Note
  • ISI Web of Science (WOS) (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#affiliazioni
  • [ 1 ] Univ Modena & Reggio Emilia, Ist Nazl Fis Mat, I-41100 Modena, Italy [ 2 ] Univ Modena & Reggio Emilia, Dipartimento Fis, I-41100 Modena, Italy [ 3 ] INFM, Lab TASC, I-34012 Trieste, Italy [ 4 ] Univ Liverpool, Surface Sci Res Ctr, Liverpool L69 3BX, Merseyside, England (literal)
Titolo
  • Variations in the lifetime of 3d hole states in ultrathin Fe films grown on Cu(100) deduced from the LMM Auger spectra of Fe (literal)
Abstract
  • The Fe LMM Auger and Auger vacancy satellite spectra of ultrathin Fe films grown on Cu(100) have been measured using photon excitation energies above and below the L-2 ionisation edge, and in coincidence with the Fe 2p(3/2) and Fe 2p(1/2) photoelectrons. A comparison of the relative intensities of the satellites and main Auger transitions indicates that the M-4,M-5 holes of L3M4,5 double hole states are localised for longer than the L-3 lifetime for the 0.3 and 10 ML coverages but have a lifetime comparable to that of L3 holes for the 1 ML coverage. The results for the 1 ML coverage are supported by the results of the coincidence experiments. The reasons for the variation in the lifetime Of M-4,M-5 holes are discussed in terms of changes in the number of Fe-Fe neighbours and the density of states at the Fermi energy in these systems. (literal)
Editore
Prodotto di
Autore CNR

Incoming links:


Autore CNR di
Prodotto
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#rivistaDi
Editore di
data.CNR.it