Mechanical Fragility and Tri-Dimensional Crack Structure in NdBaCuO Top Seeded and MultiSeeded Melt-Textured Samples (Articolo in rivista)

Type
Label
  • Mechanical Fragility and Tri-Dimensional Crack Structure in NdBaCuO Top Seeded and MultiSeeded Melt-Textured Samples (Articolo in rivista) (literal)
Anno
  • 2005-01-01T00:00:00+01:00 (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#doi
  • 10.1109/TASC.2005.848742 (literal)
Alternative label
  • M. Gombos, V. Gomis, A. Vecchione, R. Ciancio, R. Fittipaldi, A. E. Carrillo, S. Pace, and X. Obradors (2005)
    Mechanical Fragility and Tri-Dimensional Crack Structure in NdBaCuO Top Seeded and MultiSeeded Melt-Textured Samples
    in IEEE transactions on applied superconductivity (Print); IEEE-Institute Of Electrical And Electronics Engineers Inc., Piscataway (Stati Uniti d'America)
    (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#autori
  • M. Gombos, V. Gomis, A. Vecchione, R. Ciancio, R. Fittipaldi, A. E. Carrillo, S. Pace, and X. Obradors (literal)
Pagina inizio
  • 3137 (literal)
Pagina fine
  • 3140 (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#numeroVolume
  • 15 (literal)
Rivista
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#pagineTotali
  • 4 (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#numeroFascicolo
  • 2 (literal)
Note
  • ISI Web of Science (WOS) (literal)
  • Google Scholar (literal)
  • Scopu (literal)
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#affiliazioni
  • Univ Salerno, INFM Supermat, I-80181 Baronissi, SA, Italy Univ Salerno, INFM Coherentia, I-80181 Baronissi, SA, Italy Univ Salerno, Dipartimento Fis ER Caianiello, I-80181 Baronissi, SA, Italy Univ Politecn Catalunya, Dept Fis Aplicada, Barcelona, Catalunya, Spain CSIC, ICMAB, Bellaterra, Catalunya, Spain (literal)
Titolo
  • Mechanical Fragility and Tri-Dimensional Crack Structure in NdBaCuO Top Seeded and MultiSeeded Melt-Textured Samples (literal)
Abstract
  • In large TS-MTG Nd123 single-domain samples, the main lifetime limiting problem is the appearing of macroscopic fissures in the bulk, that evolve into cracks and lead to sample destruction. To analyze this phenomenon we grew single-seeded pellets and multi-seeded bars, and characterized them by XRD, PLOM, SEM and EDS. We measured inductively their superconducting properties Tc and Jc. Fissures appear to belong to micro-fissures families, parallel to the crystallographic planes. We correlate their origin to local tetra-ortho structural transition, due to spontaneous oxygenation during growth process, and their evolution toward cracks to elastic relaxation of Nd422-rich quenched liquid deposits present in the growing front concavities. MS-TSG bars growth dynamics appear to differ from pellets one. In fact, with appropriate inter-seed spacing, the absence of quenched liquid deposits near the boundaries joining adjacent domains was observed. This fact reduces mechanical fragility perpendicularly to boundaries, but does not affect the fragility along the same. Further studies are in progress on this aspect. (literal)
Editore
Prodotto di
Autore CNR
Insieme di parole chiave

Incoming links:


Prodotto
Autore CNR di
Http://www.cnr.it/ontology/cnr/pubblicazioni.owl#rivistaDi
Editore di
Insieme di parole chiave di
data.CNR.it